Issue 34, 2008

Tuning dehydrogenation temperature of carbon–ammonia borane nanocomposites

Abstract

The effect of pore size on dehydrogenation temperature and kinetics of coherent carbon–ammonia borane nanocomposites prepared by sol–gel synthesis as potential on-board hydorgen storage materials is reported.

Graphical abstract: Tuning dehydrogenation temperature of carbon–ammonia borane nanocomposites

Article information

Article type
Communication
Submitted
20 May 2008
Accepted
18 Jul 2008
First published
30 Jul 2008

J. Mater. Chem., 2008,18, 4034-4037

Tuning dehydrogenation temperature of carbon–ammonia borane nanocomposites

S. Sepehri, B. B. Garcia and G. Cao, J. Mater. Chem., 2008, 18, 4034 DOI: 10.1039/B808511K

To request permission to reproduce material from this article, please go to the Copyright Clearance Center request page.

If you are an author contributing to an RSC publication, you do not need to request permission provided correct acknowledgement is given.

If you are the author of this article, you do not need to request permission to reproduce figures and diagrams provided correct acknowledgement is given. If you want to reproduce the whole article in a third-party publication (excluding your thesis/dissertation for which permission is not required) please go to the Copyright Clearance Center request page.

Read more about how to correctly acknowledge RSC content.

Spotlight

Advertisements