Preparation of colloidal silver dispersions by the polyol process. Part 1—Synthesis and characterization

Abstract

Modification of the polyol process has enabled the synthesis of nanometre-sized silver particles with a narrow size distribution. Dispersions of colloidal silver have been prepared by the reduction of silver nitrate in ethylene glycol in the presence of a polymeric protective agent, namely polyvinylpyrrolidone (PVP). Ageing these dispersions at 120 °C for 1 h yields systems with average particle sizes ranging from 15 to 36 nm. The amount of both precursor and protective agent was found to control the final particle size and size distribution of the colloidal silver, which exhibits a well crystallized structure.

Article information

Article type
Paper

J. Mater. Chem., 1996,6, 573-577

Preparation of colloidal silver dispersions by the polyol process. Part 1—Synthesis and characterization

P. Silvert, R. Herrera-Urbina, N. Duvauchelle, V. Vijayakrishnan and K. T. Elhsissen, J. Mater. Chem., 1996, 6, 573 DOI: 10.1039/JM9960600573

To request permission to reproduce material from this article, please go to the Copyright Clearance Center request page.

If you are an author contributing to an RSC publication, you do not need to request permission provided correct acknowledgement is given.

If you are the author of this article, you do not need to request permission to reproduce figures and diagrams provided correct acknowledgement is given. If you want to reproduce the whole article in a third-party publication (excluding your thesis/dissertation for which permission is not required) please go to the Copyright Clearance Center request page.

Read more about how to correctly acknowledge RSC content.

Spotlight

Advertisements