Modification of SBA-15 pore connectivity by high-temperature

Abstract

Two-dimensional hexagonally ordered CMK-3 carbons were synthesized using SBA-15 templates calcined at a temperature of 1153 K, whereas a disordered carbon was obtained using SBA-15 calcined at 1243 K, demonstrating that the pores connecting ordered mesopores in SBA-15 silica persist up to ca. 1153 K, but are eliminated at temperatures close to 1243 K.

Article information

Article type
Communication
Submitted
05 Dec 2000
Accepted
17 Jan 2001
First published
07 Feb 2001

Chem. Commun., 2001, 349-350

Modification of SBA-15 pore connectivity by high-temperature calcination investigated by carbon inverse replication

H. J. Shin, R. Ryoo, M. Kruk and M. Jaroniec, Chem. Commun., 2001, 349 DOI: 10.1039/B009762O

To request permission to reproduce material from this article, please go to the Copyright Clearance Center request page.

If you are an author contributing to an RSC publication, you do not need to request permission provided correct acknowledgement is given.

If you are the author of this article, you do not need to request permission to reproduce figures and diagrams provided correct acknowledgement is given. If you want to reproduce the whole article in a third-party publication (excluding your thesis/dissertation for which permission is not required) please go to the Copyright Clearance Center request page.

Read more about how to correctly acknowledge RSC content.

Social activity

Spotlight

Advertisements